Skip to content
GARUDA Shisha Charcoal Indonesia Get a Quote
Menu

Charcoal problem · Charcoal Problems

Hookah Coals That Go Out — Causes and What to Specify

Coals that go out are one of the problems users report with shisha charcoal, which buyers in the USA and Canada call hookah coals. Two of the causes sit at the factory, moisture and ash, and both can be written into a specification.

Written by
Farhan Alamsyah
Published
Updated
Moisture is checked after drying and again before packing, because a dry briquette can take up water from humid air while it waits.

Quick answer

Why do my coals die on the bowl, and what should I ask a factory to control?

A coal that goes out is most often damp or was not lit all the way through; a heavy ash layer can also smother it. At this factory coals are dried for 2 to 3 days to 3–4% moisture, and moisture is checked after the oven and at packing.

1. What you see: coals that turn black on the bowl

A coal that goes out turns black on the bowl, or will not stay lit once it leaves the burner. Users describe a coal that looked ready, then lost its glow within minutes and had to be lit again.

The complaint comes up in 33 of the 207 forum threads read for this site. For a brand it is costly, because the user blames the coal and the box, not the storage or the lighting.

Note

Thread record: the counts on this page come from 207 threads of a public hookah forum, 2012 to 2026. A count shows how often a subject comes up, not a share of users. How the record was read.

2. Causes at the factory: moisture and ash

Three causes sit at the factory and two sit after it. The factory sets how dry the coal is when it is packed and how much ash it leaves; it does not set how the coal is stored or lit.

Causes of shisha charcoal that goes out, and where each one is set.
CauseWhere it is setWhat you see
Moisture left after drying At the factory, in the drying ovenThe coal is hard to light and dies on the bowl
Moisture taken in before packing At the factory, between the oven and the packing tableSome cartons light well and others do not
High ash At the factory, by the shell charcoal and the grade orderedA thick ash layer forms and the glow fades under it
Damp storage After the container leaves the factoryCoals from an opened or damaged carton go out
A coal not lit all the way through At the burnerThe coal is black at its core when it is moved

Definition

moisture content

Moisture content is the share of water in a charcoal briquette, by weight.

A heavy ash layer is a separate problem with its own page: too much ash from the coals. Damp taken in at sea or in storage, and the white spots it can leave, are on the page about damp coals and white spots. This page gives no advice on lighting or burners.

Oven drying removes the water that the binder paste brought into the briquette; a coal that leaves the oven damp is hard to light and may go out.

3. What this factory checks: moisture twice, burn test three times

The factory dries its coals for 2 to 3 days in the drying ovens, to 3-4% moisture and checks moisture twice. The second check matters as much as the first: a dry coal can take up water from humid air while it waits to be packed.

Checks this factory declares against coals that go out, with the stage of each.
CheckWhen it is doneWhat it catches
Moisture After the oven and at packingA coal that left the oven damp, or took up water afterward
Burn test Before the oven, after the oven and after packingA coal that burns at a low temperature, smokes or will not hold its glow
Ash Stage not declared yetA batch that leaves too much ash

A batch is rejected for smell, low burning temperature, cracks, splits, smoke and high ash. Where each check sits in the process is set out under the six checks and their stages, and the drying step itself under how the coal is made here.

A drying oven for charcoal briquettes circulates hot air from a burner around the trays until the briquettes reach their target moisture.

4. What to check when the container arrives

Check for damp before the load is put away, while the cartons still show what happened on the way. The four checks below need no laboratory.

  1. Step 1

    Look at the cartons

    Check for damp first. Stained, soft or swollen master cartons show that water reached the load. Photograph them before they are opened.

  2. Step 2

    Open cartons from several places

    Sample the whole load. Take cartons from the door end, the middle and the far end of the container, and check that each inner bag is closed and whole.

  3. Step 3

    Break a few pieces

    Look at the core. A piece that is softer or visibly damp at its core did not dry through.

  4. Step 4

    Burn a few pieces from each carton

    Use one method for all. Light them the way you always do and compare them with your reference box from the last container. Record the result on video.

The inner plastic bag is what keeps humid air away from the coal after it leaves the factory, so a torn bag explains a damp carton. The formats are described under how the packing protects against damp. To prevent the problem in the next order, write the moisture target and the grade into the specification sheet for your order.

The inner plastic bag is the barrier between shisha charcoal and humid air on the way from the factory to the customer.

5. If coals go out: claim within 14 days of arrival

The factory accepts a claim within 14 days after arrival. Send photos and videos of the cartons as opened and of the coals going out; the factory investigates and, if the fault is its own, compensates with a discount or with free charcoal in the next batch.

Important

The factory keeps 25 kg from each container order for 1 year, and compares it with what you received. The terms and what to send for each problem are on the page about making a quality claim.

If your present supplier's coals go out, name the problem in the quote form below or on the quote request page, so the reply states the moisture target and the checks for your order.

Questions and answers

Why do hookah coals go out on the bowl?
Most often the coal is damp or was not lit all the way through; a heavy ash layer can also smother it. Moisture and ash are set at the factory. Storage and lighting are not.
What moisture should I specify for shisha charcoal?
This factory dries its coals for 2 to 3 days to 3–4% moisture and checks moisture after the oven and again at packing. Write the moisture target for your order on the specification sheet.

Get a dated quote for your container

Fill in the order fields. The export sales desk replies by email with the price, the load and the validity date of your quote.

  1. Why we ask: Quotes, parcels and export papers are made out to a company.

  2. Why we ask: Papers, labels and the route depend on where the container is unloaded.

  3. Why we ask: The port sets the route the quote is planned on.

  4. Why we ask: Each size has its own mold, count per kilogram and container load.

  5. Why we ask: The grade sets the ash target your quote refers to.

  6. Why we ask: Full packaging and bulk are two columns of the price list.

  7. Why we ask: Printed boxes have their own minimum and add time to the order.

  8. Why we ask: The factory sells full containers only, and the load differs by size.

  9. Why we ask: Repeat orders can be planned into production ahead of time.

  10. Why we ask: The term decides which costs sit inside the price and which stay with you.

  11. Why we ask: The reply names the check that controls it.

  12. Why we ask: What your customers say about it helps us answer the right question.

  13. Why we ask: The reply is addressed to a person.

  14. Why we ask: Every reply goes to this address.

  15. Why we ask: Used only when an email does not get through.

The reply comes by email to the address you enter.